6010 and 7010 downhill has been the traditional way of welding pipe under API 1104 for many years.
But higher strength pipe is being used now that requires low hydrogen electrodes to be used for root, fill, and cap passes.
7016 is a low hydrogen electrode and is similar to 7018 but has less iron powder which makes it slightly easier for open root welds.
In this video, my friend Andrew Cardin shows his technique and settings for welding an open root using 7016 low hydrogen rod.
For even more options, check out my Amazon recommended products page at https://www.amazon.com/shop/weldingtipsandtricks
Follow Welding Tips & Tricks on social media to see what I’m up to:
Instagram: https://goo.gl/AncnFa
Facebook: https://goo.gl/e2TtXC
Join the discussion with thousands of welders at the Welding Tips & Tricks forum
http://forum.weldingtipsandtricks.com