In this guide, we'll walk you through the step by step on how to write a welding procedure specification and procedure qualification record by giving you a real-life example of welding requirements that follows AWS D1.1!
In this video you will learn:
🔍 The key welding variables defined in a WPS, including welding process, base materials, filler metals, joint design, welding position, heat treatment and variables.
🛠️ Discussion of Essential, Supplementary Essential and Non-Essential Variables
🔍 Testing the coupon and its acceptance criteria for procedure qualification
Timestamps below:
0:26 - Introductory elements of the form
1:33 - Joint Design
2:01 - Base Metal
8:21 - Filler Metal
10:08 - Supplementary Essential Variables Explanation
12:58 - Shielding Gas
14:34 - Preheat
17:04 - Welding Position
18:47 - Electrical Characteristics
19:52 - Welding Technique
20:41 - PWHT
21:07 - Qualification Testing Requirements
🚀 Don't forget to hit that "Subscribe" button and ring the notification bell so you never miss an update from Hardhat Learning! Join our community of welding enthusiasts for more informative videos like this one.
Follow me on Linkedin for more: https://www.linkedin.com/in/joemar-ancheta-34bb16165/
#Welding #WPS #PQR #WeldingVariables #Welding101 #WeldingTutorial #WeldingTips #Metalwork #WeldingCommunity #aws