More info/ an Schedule
My Schedule for The Blu tit is
1. 222c/hr 677c. 30min
2. 333c/hr 796c. (804c) 12 min hold
3. 999c/hr 482c 1 hr
4. 83c/ hr. 371c End
I have a Skutt 14 kilm
( my top temp is only 796c an a hold for 10 min)
But you know your oven Kiln if it needs more heat for a full fusing,
then you should probably use 804c hold time In 10 min
Her the link to Bullseye / and reactiv topic:
https://www.bullseyeglass.com/reactive-potential-of-bullseye-glass/
I buy the pen in Denmark from Anla glass here is the link and unfortunately I do not know a place in the US where they can be bought
https://www.anlaglas.com/shop/figuro-konturmaling-sort-1324p.html
Warmglass.UK have these glassline pens
https://www.warm-glass.co.uk/search?filter.p.m.custom.colour=Black&sort_by=relevance&type=product%2Carticle%2Cpage&options%5Bprefix%5D=last&q=pens
maybe they can be used to achieve the same result
Hope that was of some help.
I am a Danish glass artist🇩🇰
Welcome to my creative universe, where passion overlaps with technique. Discover the captivating world of glass art, as I explore the fascinating process of fusing glass, creating unique, handcrafted pieces. Subscribe for tutorials, project insights, and a behind-the-scenes look at this mesmerizing craft.
Get in touch
⭐️website: www.glglas.dk
⭐️ https://www.facebook.com/glhoff
⭐️Instagram: grethelisbaumann